Queen’s Propulsion Laboratory develops additively manufactured Kelvin Mk1 liquid rocket engine

ApplicationsNews
July 7, 2025
Students at Queen’s University Belfast have additively manufactured parts for a liquid rocket engine (Courtesy Queen’s University Belfast)
Students at Queen’s University Belfast have additively manufactured parts for a liquid rocket engine (Courtesy Queen’s University Belfast)

Students at Queen’s University Belfast have reached a major milestone for Northern Ireland’s space sector with the development of the Kelvin Mk1 liquid rocket engine. The project was Led by Queen’s Propulsion Laboratory (QPL) and is said to be the region’s first student-designed engine of its kind.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Laser Prototypes Europe (LPE) sponsored the project, additively manufacturing the engine’s combustion chamber and injector head, followed by heat-treatment and post-processing, at the company’s Belfast facility.

The chamber was produced via Laser Beam Powder Bed Fusion (PBF-LB) AM in AlSi10Mg aluminium, selected for its light weight and high thermal conductivity. The component features internal cooling channels and was built as a single piece, eliminating stress-prone welds and joints. Post-processing included full depowdering, heat treatment, and surface finishing to meet aerospace-grade standards.

The team at Queen’s University Belfast has developed the Kelvin Mk1 liquid rocket engine (Courtesy Queen’s University Belfast)
The team at Queen’s University Belfast has developed the Kelvin Mk1 liquid rocket engine (Courtesy Queen’s University Belfast)

“Additive Manufacturing was the right solution for this engine, not just for its complexity, but because it enabled speed, precision, and performance in a single process,” explained Patrick Walls, Engineering Director at LPE. “We’re proud to support such an ambitious and capable team, and to contribute to a project that represents the next generation of propulsion technology coming out of Northern Ireland.”

Founded in 2023, QPL is Northern Ireland’s largest student rocketry team and gives students real-world experience in design, manufacturing, and testing of propulsion systems. Powered by isopropyl alcohol and nitrous oxide, the Kelvin Mk1 engine is scheduled for hot fire testing on July 10, 2025, at the Westcott Space Cluster, as part of the UK’s Race2Space competition.

The QPL team chose metal Additive Manufacturing for its design flexibility, speed, and part consolidation, critical factors that allowed more time for engine testing and integration. Working with LPE also gave the students valuable experience in designing for additive processes.

“Metal 3D printing gave us greater design freedom, faster manufacturing, and fewer parts,” said a QPL spokesperson. “LPE’s support throughout the project was invaluable, and the finished chamber exceeded our expectations.”

A full Q&A with the QPL team, covering their design approach and lessons learned from the manufacturing process, is available here.

www.laserproto.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
July 7, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap