Correlation with 3D analysis. Micro-CT scanning alone struggled to resolve fine-structured Type 2 porosity. Combining LAM SEM with 3D tomography on the Helios 5 PFIB DualBeam confirmed critical voids, enhancing volumetric analysis (Courtesy Thermo Fisher Scientific)
Correlation with 3D analysis. Micro-CT scanning alone struggled to resolve fine-structured Type 2 porosity. Combining LAM SEM with 3D tomography on the Helios 5 PFIB DualBeam confirmed critical voids, enhancing volumetric analysis (Courtesy Thermo Fisher Scientific)

In a recent release, Franz Kamutzki, Senior Account Manager at Thermo Fisher Scientific Inc, Waltham, Massachusetts, USA, explored how engineers and researchers can best combine electron microscopy (EM) and micro-computed tomography (microCT) to gain deeper insights into materials at different length scales.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Kamutzki highlighted the technique through the study of functionally gradient materials (FGM), which feature a continuously variable directional composition and structure to enhance performance. These materials are particularly valuable in industrial applications required to withstand extreme stresses (e.g. aerospace components and high-performance coatings). Characterisation of FGMs is necessarily challenging, as their continuous compositional changes require a multi-analytical approach to ensure no variations are overlooked.

Analytical techniques and combined approaches

Each analytical technique provides unique and complementary insights, explains the author. Electron microscopy delivers nanometre-scale resolution, offering detailed information about a material’s surface structure, composition and microstructure. This makes it useful for studying fine structural details that influence material performance.

MicroCT, meanwhile, excels at non-destructive 3D imaging of larger samples, revealing internal features such as porosity, cracks and density variations. While its resolution is lower than EM, it provides a macroscopic perspective that allows researchers to understand how internal structures and defects are distributed throughout a material.

By integrating EM and microCT, engineers and researchers can achieve a multiscale understanding of materials that neither technique can deliver in isolation. Bridging the gap between macro- and nanoscale analyses allows for comprehensive visualisation, with MicroCT’s 3D imaging maps showcasing large-scale defects, with EM adding detailed insights into smaller features such as grain structures and elemental composition.

AI-assisted segmentation sped up analysis, with deep learning quickly identifying and segmenting porosity features, improving overall assessment efficiency (Courtesy Thermo Fisher Scientific)
AI-assisted segmentation sped up analysis, with deep learning quickly identifying and segmenting porosity features, improving overall assessment efficiency (Courtesy Thermo Fisher Scientific)

Combining data from both techniques also enables the accurate identification of defect locations, sizes and types. The insights gained from this hybrid approach can help engineers to refine manufacturing processes, thus improving material properties and performance.

Kamutzki used cold sprayed additively manufactured copper-nickel (NiCu) alloys, used in rocket chambers, to exemplify a use case of the combination technique. As FGMs, using only one method of analysis could lead to engineers missing critical material property details, thus causing safety issues.

In the ‘Multi-scale Characterization of Functionally Gradient Bimetallic Ni-Cu CSAM Alloys’ lecture presented at the 4th Symposium on Materials and Additive Manufacturing, researchers outlined a methodology for combining the two techniques to best achieve a complete picture of materials.

Yorston et al employed MicroCT to visualise porosity distribution in 3D, revealing trends such as increased pore density in nickel-rich regions. Meanwhile, the team’s EM provided nanoscale data on defect morphology and elemental distribution, uncovering smaller defect classes that microCT could not detect. These insights informed adjustments to the alloy composition and processing parameters, ultimately enhancing material reliability.

Adoption barriers

In any industries that use additively manufactured alloys such as aerospace, automotive and energy, a combined microscale analysis approach ensures a thorough understanding of material properties. In these cases, the hybrid approach can help to accelerate iterative development and reduce failure rates.

Despite its potential, however, the widespread adoption of combined EM and microCT analysis faces challenges. For instance, in industrial applications where operators are not necessarily experts in specific microscopy techniques, this approach may be perceived as overly complex. Others may question its scalability for routine industrial use that requires the analysis of thousands of samples

In his paper, Kamutzki noted the suitability of Thermo Fisher Scientific’s Arizo software in overcoming these barriers by adopting a combined data correlation/visualisation approach regardless of scale or modality. Avizo provides digital imaging-based workflows to facilitate materials characterisation and quality control from a single environment. The software offers advanced automation capabilities, allowing the creation of repeatable, reliable workflows to conduct analysis at scale.

The inclusion of artificial intelligence may enable engineers who aren’t confident with image processing to save time on complex analysis while ensuring results consistency. In addition, Thermo Fisher’s dedicated support team, training sessions and how-to guides work to reduce the learning curve for non-expert operators.

By bridging the gap between these two methods, Avizo makes the combined power of microCT and EM both practical and scalable, in an effort to drive faster, more informed decision-making in materials analysis.

www.thermofisher.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
NewsSoftware
June 11, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap