Plansee acquires Incus Hammer Evo35 for refractory metal Additive Manufacturing

EquipmentNews
March 10, 2025
Plansee has acquired a Hammer Evo35 unit from Incus (Courtesy Incus)
Plansee has acquired a Hammer Evo35 unit from Incus (Courtesy Incus)

Plansee, headquartered in Reutte, Austria, has announced its acquisition of a Hammer Evo35 lithography‐based metal manufacturing (LMM) machine from Incus GmbH, Vienna. The addition is intended to strengthen its industrial metal Additive Manufacturing offering.

The Hammer Evo35 is a redesign of Incus’s Hammer Lab35, offering Incus’s LMM AM technology in tandem with better production capabilities and industrial performance than the earlier machine.

“After intensive material development efforts, we have proven the capabilities of the technology for refractory metal printing,” said Dr Gerald Mitteramskogler, CEO of Incus. “It is a great pleasure to provide our technology to such a prestigious organisation as Plansee SE.”

“With this technology, Plansee SE is expanding its capabilities for producing high-resolution parts and components out of refractory metals and their alloys using 3D printing,” added Dr Dirk Handtrack, Project Manager at Plansee SE. “This underlines the excellent and trusting cooperation between the two companies.”

www.incus3d.com

www.plansee.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
EquipmentNews
March 10, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap