Amazemet to unveil Powder2Powder atomiser for recycling metal powders at Formnext 2024

The key challenges addressed by the new Powder2Powder technology (Courtesy Amazemet)
The key challenges addressed by the new Powder2Powder technology (Courtesy Amazemet)

Amazemet Sp Zoo, based in Warsaw, Poland, will introduce its new Powder2Powder (P2P) atomisation machine at Formnext 2024. The P2P system is reported to provide a versatile solution for recycling metal powders, and manufacturing custom pre-alloy powders directly from powder feedstock.

The technology combines plasma processing and ultrasonic atomisation to transform irregular or oversized particles into highly spherical, satellite-free powders optimised for Additive Manufacturing. Unlike plasma spheroidisation, the P2P technology allows powder size to be independent of the initial feedstock, reportedly making it the only technology capable of direct atomisation of pulverised titanium feedstock.

“The Powder2Powder system goes beyond recycling,” explains Łukasz Żrodowski, inventor and CEO of Amazemet. ”It gives manufacturers the ability to customise powder compositions, improve powder sphericity, and optimise particle size distribution, solving critical issues in the AM industry. We’re excited to debut this at Formnext 2024, where we’ll showcase how it can enhance the efficiency and sustainability of powder-based manufacturing.”

Atomisation of TiMo alloy via Powder2Powder technology a) feedstock material - blend
of pure Ti and Mo elements, b) as atomised TiMo alloy, c) Particle Size Distribution of feedstock and TiMo alloy, d) sphericity of feedstock and TiMo alloy (Courtesy Amazemet)
Atomisation of TiMo alloy via Powder2Powder technology a) feedstock material – blend of pure Ti and Mo elements, b) as atomised TiMo alloy, c) Particle Size Distribution of feedstock and TiMo alloy, d) sphericity of feedstock and TiMo alloy (Courtesy Amazemet)

Extensive trials using +200 µm oversize and irregular Ti alloy powders have reportedly shown exceptional results with the P2P system. Operating at a frequency of 40 kHz, the system consistently achieved a powder morphology with an aspect ratio (D50) exceeding 0.95. The particle size distribution (PSD) was precisely controlled, producing powders with D90 < 80 µm and yielding particles <63 µm and ≥80%. Nearly 97% of the resulting powder was suitable for AM processes, including Laser Beam Powder Bed Fusion (PBF-LB), Directed Energy Deposition (DED), and Electron Beam Powder Bed Fusion (PBF-EB), highlighting the machine’s potential to enhance sustainability in metal powder production.

Additionally, the P2P system can process blends of elemental powders, creating pre-alloyed materials tailored to exact chemical compositions. This capability makes it invaluable for both research and industrial applications. Tests conducted with Ti and 10% wt. Mo elemental powders showed that both refractory elements formed homogeneous alloy powders during processing. Set for release in Q1 2025, this patented technology addresses two critical challenges in the AM industry – upcycling of powder waste and custom powder production -delivering advanced functionality that surpasses traditional recycling methods.

Key features include:

  • Particle size distribution control: The system adjusts the particle size distribution (PSD), transforming under- and oversized particles into powder optimised for PBF-LB, DED, and other AM techniques.
  • Powder morphology: By combining plasma-based technology for melting feedstock powders with ultrasonic atomisation to refine particle morphology, the system transforms irregular powders into highly spherical, satellite-free particles, enhancing performance in AM processes.
  • Powder alloying: Blends of elemental powders or commercial alloys with minor alloying element additions can be used as feedstock for atomisation. Unlike in EIGA or plasma atomisation, new alloys can be rapidly developed without preprocessing, electrode casting, or wire drawing.
  • Multi-material capability: The system handles a wide range of metal powders, including steel, titanium, nickel, refractory alloys, and high-entropy alloys (HEAs), with the ability to create powders that meet specific AM feedstock requirements.
  • Sustainability and efficiency: By converting otherwise unusable powders into AM-ready material, the P2P system minimises waste and supports sustainable manufacturing practices.

Formnext 2024 attendees will be the first to experience the innovative system, which offers a complete solution for both recycling and custom alloy powder production. Visit Amazemet in Hall 12, E61.

powdertopowder.amazemet.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

 

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap