MIM operation reduces product lead time to by up to 13 weeks with ExOne
Metal Injection Moulding (MIM) company MIMtechnik GmbH, Schmalkalden, Germany, is reducing the lead time for prototype MIM products to as little as one week using Binder Jet Additive Manufacturing ... Read more »