Framatome opens €25M French nuclear AM centre

Framatome has officially inaugurated the Amiral Bernard-Antoine Morio de l’Isle Additive Manufacturing Centre in Romans-sur-Isère, France (Courtesy Framatome)
Framatome has officially inaugurated the Amiral Bernard-Antoine Morio de l’Isle Additive Manufacturing Centre in Romans-sur-Isère, France (Courtesy Framatome)

Framatome officially opened the Amiral Bernard-Antoine Morio de l’Isle Additive Manufacturing Centre in Romans-sur-Isère, France, on July 2. Less than a year after laying the first stone, the 6,000 m² facility, backed by a €25 million investment, is now fully operational and is producing critical spare parts for the primary circuits of French nuclear reactors.

The centre leverages MX3D’s Wire Arc Additive Manufacturing (WAAM), a wire-based Directed Energy Deposition (DED) process, to manufacture critical components with complex geometries. These include medium-sized parts such as 1-ton impellers up to massive structures weighing between 20 and 25 tons, intended for the nuclear and French defence sectors.

This strategic production hub is designed to meet the strictest safety requirements across the nuclear energy sector. Framatome states that integrating WAAM reduces raw material waste and energy consumption, while also cutting lead times compared to traditional forging.

“With the Amiral Bernard-Antoine Morio de l’Isle centre fully operational, we have entered a new era for truly large-scale Additive Manufacturing in Nuclear Energy,” said Gijs van der Velden, CEO of MX3D. “We are incredibly proud that MX3D’s WAAM systems are a core driving force inside Europe’s first nuclear facility of this scale. The opening of this facility marks a milestone in strengthening European strategic and sovereign industrial capability. It proves that large-scale metal 3D printing is ready to deliver repeatable quality for the most demanding applications in the nuclear sector and beyond.”

Framatome stated, “This centre stands as an essential lever to contribute to the performance of the nuclear sector, secure our supply chain, and reinforce our industrial sovereignty. Here, innovation takes shape and excellence is printed.”

www.framatome.com

www.mx3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap