LAYRR develops nano-coating process for metal AM powders
LAYRR, based in Abingdon, UK, has developed a high-speed surface engineering process, adapted from Physical Vapour Deposition (PVD), to modify standard metal powders at the atomic level. The approach is intended ... Read more »