Amaero secures AU$7.8 million titanium powder order

Amaero has two EIGA Premium atomisers from ALD Vacuum Technology GmbH for the production of high-quality spherical metal powders. A third is expected to be commissioned this year (Courtesy ALD Vacuum Technology GmbH)
Amaero has two EIGA Premium atomisers from ALD Vacuum Technology GmbH for the production of high-quality spherical metal powders. A third is expected to be commissioned this year (Courtesy ALD Vacuum Technology GmbH)

Amaero Ltd, McDonald, Tennessee, USA, has entered a Master Purchasing Agreement that includes a Purchase Order for titanium alloy powders with a value of AU$7.8 million.

With an increase in installations of Additive Manufacturing equipment, Amaero is reportedly experiencing strong demand for titanium alloy powders. The demand is driven by accelerating adoption of Additive Manufacturing across defence, aerospace, medical, consumer and civilian firearms markets. Powder demand for Laser Beam Powder Bed Fusion (PBF-LB) is focused on mature, high-production-rate gas- and plasma-atomised powder technologies.

With two advanced EIGA Premium atomisers commissioned and a third expected to be commissioned in June, Amaero states that it has commissioned the largest-capacity and the lowest-unit-cost US domestic production of refractory and titanium alloy spherical powders.

Defence, space and nuclear applications are also driving demand for refractory alloy spherical powders. Amaero has orders in the current quarter to atomise five different high-value refractory alloys.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Hank J Holland, Amaero’s Chairman and CEO, commented, “Commercial activity across both segments of Amaero’s business is strong. We are excited to secure a contract for titanium powder shipments in FY2027 that approximates total titanium powder sales in FY2026. We have been advancing numerous titanium powder opportunities over the past 6-12 months with several opportunities potentially exceeding 100 tonnes of annual demand. We are also advancing a strategic contract for refractory powder development that we expect to finalise by the end of the fiscal year. Finally, strong momentum in PM-HIP manufacturing and notable progress toward production contracts continues. We are excited to finish FY2026 with strong performance and expect to enter FY2027 with strong bookings and revenue visibility.”

amaeroinc.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap