Osaka Titanium Technologies receives AS9100 certification for spherical Ti alloy powder
Osaka Titanium Technologies Co., Ltd., Amagasaki, Hyōgo Prefecture, Japan, has been awarded JIS Q 9100 (AS9100) certification for its TILOP (Pre-Alloy) spherical titanium alloy powder. AS9100 is a widely ... Read more »