Researchers reduce residual PBF-LB warpage in new research
Researchers from Waseda University, Tokyo, Japan, and University of Pittsburgh, Pennsylvania, USA, have published research on warpage reduction methods when utilising Laser Beam Powder Bed Fusion (PBF-LB) ... Read more »