ExOne launches #MakeMetalGreen social media campaign
The ExOne Company, North Huntingdon, Pennsylvania, USA, has launched a new #MakeMetalGreen social media campaign in order to educate manufacturers about the sustainability benefits ... Read more »
The ExOne Company, North Huntingdon, Pennsylvania, USA, has launched a new #MakeMetalGreen social media campaign in order to educate manufacturers about the sustainability benefits ... Read more »
3D Systems, Rock Hill, South Carolina, USA, reports that its Board of Directors has named Dr Jeffrey A Graves, as the company’s new President and CEO, effective May 26, 2020. Graves brings seventeen ... Read more »
SPEE3D, headquartered in Melbourne, Australia, demonstrated its ACTIVAT3D copper coating process during a live online presentation. The company recently announced the successful development ... Read more »
Mesago Messe Frankfurt GmbH, the organiser of Formnext, reports that it still expects the event scheduled to take place in Frankfurt, Germany, from November 10–13, 2020, to go ahead. The organiser also states ... Read more »
Carpenter Technology Corporation, headquartered in Philadelphia, Pennsylvania, USA, has stated it plans to idle two of its US-based metal powder production facilities, as the company reacts ... Read more »
The Metal Powder Industries Federation (MPIF) and APMI International, the American Powder Metallurgy Institute, have launched a series of complimentary technical webinars for its members ... Read more »
Gefertec GmbH, Berlin, Germany, reports that it is expanding its metal Additive Manufacturing reach in Asia by supplying two of its 3DMP® machines to two Asian-based companies ... Read more »
Bodycote plc, headquartered in Macclesfield, Cheshire, UK, plans to open a new heat treatment facility in Elgin, Illinois, USA, reported to be a replacement for the company’s ageing facility in Melrose Park ... Read more »
Tekna, headquartered in Sherbrooke, Quebec, Canada, is launching a webinar series with the first edition focusing on ‘Powder Processing in a Circular Economy.’. The first webinar, to be presented ... Read more »
The VDMA’s Additive Manufacturing Working Group (AG AM) has released the results of a member survey it conducted in April 2020. With almost eighty members taking part, the VDMA stated that production ... Read more »
Elementum 3D, Inc, Erie, Colorado, USA, has achieved ISO 9001:2015 certification for quality management, issued through Platinum Registration, Inc., a ISO 9001 management certification firm based in Denver ... Read more »
3DEO, Inc., a metal Additive Manufacturing technology company based in Los Angeles, California, USA, has announced a 600% growth in revenues for 2019 over 2018. The company also reported a 394% ... Read more »
Additive Manufacturing consultancy Ampower, Hamburg, Germany, has released the AMPOWER Report 2020. The independent market and technology report for metal Additive Manufacturing ... Read more »
America Makes, Youngstown, Ohio, USA, is launching a series of vitual panel and networking events titled ‘Virtual Game Day Series’ in association with Wohlers Associates, Inc., Fort Collins, Colorado, USA ... Read more »
Melrose Industries PLC, UK, has released a trading update for the four months from January 1, 2020, to April 30, 2020, and reports an estimated 20% sales decrease in this period due to the impacts ... Read more »
SBI International, Hollabrunn, Austria, and Multistation SAS, Paris, France, have entered into an exclusive partnership to deliver Plasma Arc metal Additive Manufacturing to the French market. As part of the partnership ... Read more »
Dunlee, a distributor of products, solutions and services for the third-party imaging business, headquartered in Hamburg, Germany, reports that it is increasing its output of additively manufactured tungsten ... Read more »
Velo3D, Campbell, California, USA, has announced the commercial release of a manufacturing process for additively manufactured parts in aluminium F357 on its Sapphire® metal Additive Manufacturing ... Read more »
Optomec, headquartered in Albuquerque, New Mexico, USA, has announced an advancement in capability for its LENS Directed Energy Deposition (DED) Additive Manufacturing machines ... Read more »
America Makes, Youngstown, Ohio, USA, has launched its next project call to support the continued technological advantage of the U.S. Air Force (USAF). The ‘Additive for eXtreme Improvement ... Read more »