Gasbarre has received three separate orders for batch steam treaters (Courtesy Gasbarre Thermal Processing Systems)

Gasbarre Thermal Processing Systems, based in St. Marys, Pennsylvania, USA, part of Gasbarre Products Inc., has received three separate orders for batch steam treating equipment. Steam treating processes are used in many different industries and these orders will be shipped to companies that provide products to the medical, Additive Manufacturing, automotive and consumer products sectors.

The batch steam treaters produce an oxide layer that promotes corrosion and wear resistance properties and provides an attractive surface finish. The performance and quality of the surface and subsurface layers depends to a great extent on surface cleanliness and the overall (atmosphere) integrity of the equipment.

The three orders range in size from 45 cm to 76 cm diameter and 30 cm to 121 cm deep. The gross load weight capacity ranges from 136 kg to 816 kg with Gasbarre supplying the production tooling. The equipment is electrically heated and has a maximum operating temperature rating of 760℃.

www.gasbarre.com/thermal-processing-systems

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap