FIT Additive Manufacturing to add SPEE3D’s supersonic 3D deposition to its technology offering

News
September 18, 2018
FIT Additive Manufacturing to add SPEE3D's supersonic 3D deposition to its technology offering

The SP3D machine fires metal powders onto a defined spot on a material carrier at ‘three times the speed of sound’ to produce components without melting or heat (Courtesy SPEE3D)

 

FIT Additive Manufacturing Group, Lupburg, Germany, has purchased a supersonic 3D deposition (SP3D) machine produced by SPEE3D, Melbourne, Australia. According to SPEE3D, its machines can manufacture copper and other metal components in record time.

In an SP3D machine, metal powder is not spread over a surface but fired by a nozzle onto a defined spot on a material carrier. The powder particles hit that position at three times the speed of sound, with the corresponding kinetic energy, which binds them without the use of melting or heat.

The first SP3D machine will be installed by FIT late in 2018, initiating an extensive testing phase. Philip Emmerling, Research Engineer at FIT, stated, “We will focus on the functional performance of the components produced by this machine. Our first tests were promising, but much work has to be done.”

 

FIT Additive Manufacturing to add SPEE3D's supersonic 3D deposition to its technology offering

Components produced using SPEE3D’s supersonic 3D deposition process (Courtesy SPEE3D)

 

With its investment in this new type of system from SPEE3D, FIT aims to continue its transition from an additive manufacturer to a global AM research and development partner for industrial clients. “Fifteen years ago, we moved from service bureau to Additive Manufacturing with Electron Beam Melting technology. Five years ago, we started to support our clients with additive design challenges – mostly with powder bed technologies,” stated Carl Fruth, Founder and CEO of FIT AG.

“Now, new additive technologies and new players are emerging all the time. These need to be implemented on an industrial scale – independent from machine manufacturers – and we need to constantly scout the AM universe for new developments,” he concluded, while Albert Klein, CFO and CSO of FIT AG, added, “With this broad and deep approach we can support our clients in their extremely complex additive design and manufacturing problems. We are rapidly moving to additive technology partnerships rather than Additive Manufacturing.”

www.fit.technology

www.spee3d.com

News
September 18, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap