Companies & MarketsNews
November 3, 2026
GKN Aerospace has achieved Nadcap accreditation for Laser Wire Directed Energy Deposition (Courtesy GKN Aerospace)
GKN Aerospace has achieved Nadcap accreditation for Laser Wire Directed Energy Deposition (Courtesy GKN Aerospace)

GKN Aerospace’s facility in Trollhättan, Sweden, has reportedly become the first company worldwide to achieve Nadcap accreditation for Laser Wire Directed Energy Deposition (L-DED-w). The accreditation provides independent, industry-recognised validation of the company’s L-DED-w manufacturing processes and is expected to support broader industrial adoption of the technology in aerospace and defence applications.

Nadcap is an aerospace industry accreditation programme for special processes, assessing compliance with requirements for quality, traceability and process control. GKN Aerospace achieved accreditation following a comprehensive audit covering its process controls, operating procedures, personnel qualifications, equipment, material control and traceability.

GKN Aerospace has already designed, developed and delivered fully certified components produced using Additive Manufacturing, which are currently in flight. The company expects the accreditation to support the introduction of further L-DED-w applications into full aerospace production.

“Our customers are looking for trusted partners that can help industrialise advanced manufacturing technologies,” stated Sébastien Aknouche, SVP Material Solutions at GKN Aerospace. “For Additive Manufacturing, that means having robust and repeatable processes that can support the move into industrial production. Nadcap accreditation is an important step in that journey, giving us a stronger foundation for broader application of L-DED-w across aerospace and defence.”

www.gknaerospace.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
Companies & MarketsNews
November 3, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap