Metalysis secures €1M ESA funding for titanium process

Production cells at the Metalysis Discovery Centre in South Yorkshire (Courtesy Metalysis)
Production cells at the Metalysis Discovery Centre in South Yorkshire (Courtesy Metalysis)

Metalysis Ltd, Rotherham, UK, has been awarded near €1 million in funding from the European Space Agency (ESA) to develop a continuous or quasi-continuous process for titanium production using its FFC (Fray-Farthing-Chen) molten salt electrolysis technology.

The twenty-four-month project aims to scale Metalysis’ FFC process to support more sustainable bulk titanium production and strengthen Western supply chains for critical metals.

Metalysis will lead a consortium including the UK’s Lucideon Ltd, TTP plc and NCHG Ltd, along with Austria’s RHP-Technology GmbH. Covering key unit operations associated with the FFC process, the partners bring experience in ceramics processing, materials science, electrochemistry, process development and Powder Metallurgy.

The consortium will work to scale the process beyond its current batch configuration towards continuous or quasi-continuous operation. According to Metalysis, its existing GEN-3 and GEN-4 reactors are able to produce titanium powders to the metal Additive Manufacturing sector, but production volumes are currently insufficient for wider bulk titanium markets.

Other consortium partners will contribute expertise in feedstock development, process scale-up, modelling and materials consolidation.

Titanium and its alloys are widely used in space and aerospace applications due to their high strength-to-weight ratio, corrosion resistance and performance at elevated temperatures. However, supply chain resilience has become an increasing concern.

Prior to 2022, a significant proportion of the titanium sponge used by Western aerospace manufacturers was sourced from Russia, Metalysis explains. China now accounts for roughly 70% of global titanium sponge production, increasing pressure to develop alternative supply routes.

Article: Inside Nikon’s metal AM strategy
Part 2: Scaling industrial production in Long Beach
Read now

“The near €1 million from ESA to our consortium, led by Metalysis, reflects the strategic need across the space, aerospace, defence, hypersonics and wider advanced manufacturing sectors for industrial-scale production of critical metals such as titanium,” stated Nitesh Shah, CEO of Metalysis. “Scaling our technology to continuous or semi-continuous production will help strengthen Western supply of sustainable titanium, as the Metalysis FFC process is leaner, greener and cleaner than traditional manufacturing routes.”

The conventional Kroll process used for titanium production is energy-intensive and involves multiple processing stages, including melting and thermomechanical processing. The process also relies on chlorine gas and generates hazardous waste streams.

Metalysis stated that its FFC process offers a potential alternative through direct electrochemical reduction of metal oxides in molten salt. This approach enables titanium and titanium alloys to be produced in the solid state, avoiding several melting and thermomechanical processing steps associated with conventional production routes. The company also noted that combining the process with Powder Metallurgy routes could enable near-net-shape component production, potentially reducing material waste and energy consumption.

“Titanium is essential for space exploration and satellite manufacturing, and establishing a secure, environmentally responsible supply chain is vital for the long-term competitiveness of our space sector,” explained Matthew Cook, Head of Space Exploration at the UK Space Agency.

The FFC process was originally developed at the University of Cambridge in 1997 as a lower-cost and more energy-efficient route for producing titanium and other metals.

Tim Abbott, Director of Commerce at Lucideon, added, “By combining our materials and processing expertise with the facilities available at The AMRICC Centre, we aim to help develop scalable feedstock production processes that enable more efficient and sustainable manufacturing solutions.”

David Pooley, Project Leader at TTP plc, stated that the project represents “a major step towards securing a sustainable titanium supply chain for the UK and Europe,” noting that the company will apply modelling and pilot-scale data to support the transition to reliable large-scale production.

Erich Neubauer, General Manager at RHP-Technology, said the company will contribute its expertise in advanced materials and consolidation processes “to optimise titanium powder and bulk component properties.”

Nick Weeks, Director of NCHG Ltd, noted that the programme highlights the importance of developing more resilient and lower-impact supply chains for critical materials across UK and European industry.

www.metalysis.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap