voestalpine’s new special steel plant begins testing

July 6, 2022

The new plant at voestalpine is expected to produce 205,000 tons of special steel annually (Courtesy voestalpine)
The new plant at Kapfenberg (Courtesy voestalpine)

Four years after its groundbreaking ceremony, the special steel plant at voestalpine’s site in Kapfenberg, Austria, is now complete. The facility – intended to annually produce 205,000 tons of special steel, some of which will be metal powder for AM – is said to represent a technical milestone for the voestalpine Group’s High Performance Metals Division in terms of digitalisation and sustainability.

The plant replaces the existing voestalpine Böhler Edelstahl GmbH & Co KG plant in Kapfenberg, and is in addition to its traditional steel products, will produce metal powders for Additive Manufacturing. The first facilities are already undergoing testing.

The project progressed throughout the COVID-19 pandemic, although delays in the delivery of key equipment led to project completion being pushed back by over a year. At the same time, voestalpine calculates that due to the difficult framework conditions, costs are expected to rise by around 10% to 20% over the initial planned investment of €350 million.

“As the plant starts operating in fall 2022, initially with intermittent parallel operations using the existing electric steel mill, we can supply our customers with even better material qualities to further expand our global market leadership in tool and special steels,” stated Franz Rotter, member of the Management Board of voestalpine AG and Head of the High Performance Metals Division. “Our heartfelt thanks go to our dedicated employees at the site whose flexibility and extensive expertise will make this successful start-up possible.”

“The new special steel plant will set new global benchmarks in sustainability and energy efficiency,” added Rotter. “This makes this investment an integral part of our overall sustainability strategy.”

www.voestalpine.com

The new plant at voestalpine is expected to produce 205,000 tons of special steel annually (Courtesy voestalpine)

In the latest issue of Metal AM magazine

Download PDF
 

Extensive AM industry news coverage, as well as the following exclusive deep-dive articles:

  • Transforming access to medical implants with PrinterPrezz
  • Lessons from 2021’s Olympic bike crash
  • Xerox liquid metal AM
  • Additive Manufacturing for oil, gas and maritime
  • Multi-material metal parts by Powder Bed Fusion
  • Findings from Wohlers Report 2022
  • The challenge of grain size: X-ray powder diffraction analysis of parts made by metal AM

The world of metal AM to your inbox

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Sign up

News from the industry…

    News from the industry…

    Discover our magazine archive…

    The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

    • Reports on visits to leading metal AM part manufacturers and industry suppliers
    • Articles on technology and application trends
    • Information on materials developments
    • Reviews of key technical presentations from the international conference circuit
    • International industry news

    All past issues are available to download as free PDFs or view in your browser.

    Browse the archive

    qweqw

    Looking for AM machines, metal powders or part manufacturing services?

    Discover suppliers of these and more in our comprehensive advertisers’ index and buyer’s guide, available in the back of Metal AM magazine.

    • AM machines
    • Process monitoring & calibration
    • Heat treatment & sintering
    • HIP systems & services
    • Pre- & post-processing technology
    • Powders, powder production and analysis
    • Part manufacturers
    • Consulting, training & market data
    Download PDF
    Share via
    Copy link
    Powered by Social Snap