Freemelt receives patents in China and Japan for Spot Preheating method
Freemelt AB, Mölndal, Sweden, has been granted patents in both China and Japan for its method of ‘Spot Preheating’ that consists of the point-by-point preheating of each powder layer in the Powder Bed Fusion ... Read more »