Penn State University research lab acquires SPEE3D metal AM machine
The Applied Research Laboratory of Penn State University, Pennsylvania, USA, a US Department of Defense designated University Research Centre, has acquired a LightSPEE3D Cold Spray metal Additive Manufacturing ... Read more »