AIM3D’s Voxelfill principle overcomes inhomogeneous strength issues with cross-layer filling strategy
AIM3D GmbH, Rostock, Germany, has developed a new process for sustainably improving the strength properties of an additively manufactured component. The company’s patent-pending Voxelfill technology ... Read more »