VBN’s Vibenite 350 shows promise for implant use following biocompatibility and wear-resistant tests
VBN Components, based in Uppsala, Sweden, has reported that the first in-vitro biocompatibility tests of its additively manufactured Vibenite 350 have been conducted within the competence centre AM4life. ... Read more »