University of Sheffield uses solid-state processing to transform surplus Al powders
Researchers from the Sheffield Titanium Alloy Research (STAR) group, part of the UK’s University of Sheffield, have partnered with ECKART GmbH, Schluechtern, Germany, to convert surplus aluminium alloy ... Read more »