Titomic’s TKF technology to be used on metal parts for Airbus
Titomic Ltd, Melbourne, Australia, has entered into an agreement with Airbus in which Titomic’s patented Titomic Kinetic Fusion (TKF) Additive Manufacturing technology will be used to demonstrate ... Read more »