Wayland Additive’s Calibur3 achieves superior Ti6Al4V performance
Wayland Additive, located in Huddersfield, UK, has announced that Ti6Al4V Grade 5 titanium processed on its Calibur3, using NeuBeam technology, has officially met and exceeded international Additive ... Read more »