Molymet invests in plasma atomisation technology for rhenium and molybdenum powders
Molymet, San Bernardo, Chile, has acquired plasma atomisation equipment to enable the production of highly spherical powders of rhenium, molybdenum, and their alloys, all specifically designed for industrial ... Read more »