Netherlands Cancer Institute implants its first AM titanium jaw from M3DT

The Mobius 3D Technologies titanium jaw is bespoke based on patient MRI & CT scans (Courtesy the Antoni van Leeuwenhoek/Netherlands Cancer Institute)
The Mobius 3D Technologies titanium jaw is bespoke based on patient MRI & CT scans (Courtesy the Antoni van Leeuwenhoek/Netherlands Cancer Institute)

Following four years of research, an additively manufactured titanium mandible was successfully implanted by the Antoni van Leeuwenhoek Hospital/Netherlands Cancer Institute (NKI) in a patient with head and neck cancer. The mandible was entirely additively manufactured using 3D MRI & CT scans of the patient based on the joint research between the Antoni van Leeuwenhoek/NKI and Mobius 3D Technologies (M3DT), Velsen-Noord, the Netherlands.

Typically, tumours in and around the mandible are treated by removing part of the mandible and replacing it with bone from elsewhere in the body. The problem with this reconstruction method, however, is that the bones are said to break in about 40% of the cases and/or the screws by which the bones are attached become loose. This has necessarily drastic consequences for the patient.

This titanium mandible is much stronger than bone, with forces optimally distributed via a mesh structure within the implant which enables that strength whilst remaining lightweight for the patient. This additively manufactured implant also features a new fastening technique which is intended to ensure that the implant remains in place, and because the implant is bespoke, the jaw fits the patient well enough to enable vital functions like talking, drinking and eating.

The tools used by the surgeon in the operation are also patient specific, enabling a simpler, shorter operation and, thus, minimising the risk of complications.

www.avl.nl

www.mobius3dt.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap