Matsuura Machinery USA launches metal AM production services

Matsuura’s LUMEX Avance-25 metal Additive Manufacturing machine is said to minimise mould assembly; create superior mould performance; reduce lead time, and perform high-precision machining without EDM (Courtesy Matsuura Machinery USA, Inc.)

Matsuura Machinery USA, Inc., the US subsidiary of Matsuura Machinery Corporation, based in St. Paul, Minnesota, reports that it now offers quick-turn prototyping, producing a wide range of metal additively manufactured parts, including unique functional prototypes and low to mid-volume production runs.

“Due to unprecedented customer interest and demand, Matsuura’s Metal Additive Manufacturing Service Bureau is now providing the production of 3D Metal printed and machined parts,” stated Tom Houle, Director, LUMEX, NA.

The company explains that with its LUMEX Avance-25 and Avance-60 metal AM machines, the production of high-volume mould components with conformal cooling and integrated porous venting will minimise the need for traditional EDM processes and provide significant savings to the production of moulded plastic components. Customers can lower their capital equipment investments for tooling and moulding machines while reducing mould cavitation requirements and accelerating Return on Investment (ROI).

“Products and shapes previously impossible to manufacture (including ultra-deep ribs, 3D mesh, hollows, free-form surfaces, and porous structures) can now be produced using the LUMEX Technology,” Houle added.

Matsuura USA established its Additive Manufacturing Center to promote the use of metal AM parts as a solution to continuing supply chain challenges and delays.

Houle continued, “The LUMEX team in our Additive Manufacturing Center, along with our collaboration with the Customer Solutions team and machine designers in Japan and Germany, will help customers quickly realise the benefits of Additive Manufacturing. Our team’s insight into the process and the technology, will assist in modification of your traditional designs into suitable 3D Metal Printing.”

Matsuura customers are reported to be seeing the value that comes with implementing AM technology, with multiple customer case studies showing 25% to 45% reductions in cycle time reductions.

“Metal 3D Printing can benefit Tooling, Injection Molding, CNC Machining, and Die Casting processes and operations.  We will work with you throughout the entire 3D printing process, including through the design to enable our customer’s to fully realise the benefits throughout the life of their products,” Houle concluded.

www.matsuurausa.co

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap