ExOne reveals new X1 25PRO metal AM system and announces Kennametal as beta customer

News
May 23, 2019
ExOne reveals new X1 25PRO metal AM system and announces Kennametal as beta customer

The ExOne Company revealed its new X125PRO beta system at Rapid + TCT 2019 (Courtesy ExOne)

 

The ExOne Company, a provider of Additive Manufacturing systems and services, headquartered in North Huntingdon, Pennsylvania, USA, has revealed its new X1 25PRO™ metal Additive Manufacturing beta system at Rapid + TCT 2019, Detroit, Michigan, USA, from May 20–23. The company also announced Kennametal Inc., a supplier of tooling and wear resistant solutions, located in Latrobe, Pennsylvania, USA, as a beta customer.

During the beta period ExOne states that Kennametal will have the opportunity to evaluate the X1 25PRO system and trial new materials and processes. According to ExOne, the high-resolution production machine is capable of Additive Manufacturing metal, ceramic, and other advanced material parts directly, as well as standard industry powders utilised in Metal Injection Moulding (MIM) and other Powder Metallurgy (PM) processes.

“We see Binder Jet technology as a key enabler for our differentiated, high-performance wear materials, such as tungsten carbide and Kennametal Stellite™ alloys,” stated, Sherri McCleary, Director of Business Development Additive at Kennametal. “Kennametal is uniquely qualified to supply these additive materials and components, and we’re pleased to collaborate with ExOne on cutting-edge technology with the potential to help us advance from prototyping to serial production.”

John Hartner, Chief Executive Officer at ExOne, commented, “Working with innovative, global companies like Kennametal is another important step towards integrating industrial 3D printing into existing and new production lines. We are excited to bring Kennametal on as a beta user and and look forward to beginning the testing programme.”

www.exone.com  |  www.kennametal.com

 

News
May 23, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap