Fraunhofer demonstrates vibration-eliminating support structures for post-processing of metal AM parts

News
July 24, 2018
Fraunhofer demonstrates vibration-eliminating support structures for post-processing of metal AM parts

Fraunhofer IPT and ILT have developed a support structure design which is said to eliminate vibration during post-processing (Courtesy Fraunhofer IPT)

 

The Fraunhofer Institutes for Production Technology (IPT) and Laser Technology (ILT), Aachen, Germany, have developed a new design for support structures which is said to eliminate part vibration during post-processing operations such as milling or grinding. Milling operations conducted on thin-walled parts in particular often cause vibrations which can negatively impact both part accuracy and machining time.

As a rule, metallic components manufactured using Powder Bed Fusion (PBF) processes are designed with a larger-than-usual oversize to allow for functional surfaces to be finished in milling operations, since this is the only way of ensuring that all of the surface tolerances and quality requirements can be met. Thin-walled parts are particularly prone to vibration in the course of the machining and material removal operations, and this can result in poor surface quality or even render the components unusable.

 

Fraunhofer demonstrates vibration-eliminating support structures for post-processing of metal AM parts

Support structures for the reduction of vibration during milling (Courtesy Fraunhofer IPT)

 

Fraunhofer IPT and ILT’s new support structures are said to increase the stiffness of susceptible areas of AM parts and thereby reduce vibrations during post-processing. They can also be removed with relatively little effort in the course of the surface finishing operation. Parts stabilised in this way can reportedly be manufactured in higher quality in less time, and with lower level of tool wear.

www.ipt.fraunhofer.de

www.ilt.fraunhofer.de

News
July 24, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap