BEAMIT adds metal AM production capacity and new materials

News
May 18, 2018
BEAMIT adds metal AM production capacity and new materials

AM components manufactured by BEAMIT SpA

 

Italy’s BEAMIT SpA, Fornovo Taro (Parma), reports that it is further expanding its Additive Manufacturing production capacity with a new EOS M400-4 system. With a build volume of 400 x 400 x 400 mm, the new system will be dedicated to the production of AlSi10Mg parts. This new machine will be installed in early June as part of an agreement that was been signed last year with EOS.

The company currently operates 22 metal AM machines, producing parts from a portfolio of 12 materials. The company already uses EOS M400-4 systems for Ti6Al4V and Hastelloy x and the addition of AlSi10Mg is, it was stated, based on customer demand.

BEAMIT is a leading supplier of metal-based AM production components. The company serves a number of industrial sectors, from biomedical and motorsports to the aerospace and energy sectors.

www.beam-it.eu

News
May 18, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap