New low cost system offers easy access to metal Additive Manufacturing

News
November 7, 2016

 

New low cost system offers easy access to metal Additive Manufacturing

The SLM unit for Additive Manufacturing of stainless steel components is particularly suitable for entry-level users (© Photo Fraunhofer ILT, Aachen, Germany)

Germany’s FH Aachen and Fraunhofer Institute for Laser Technology ILT have announced the development of a new low-cost Selective Laser Melting (SLM) unit that will be displayed at this year’s formnext, Frankfurt, Germany, November 15-18, 2016. Built jointly with the GoetheLab at FH Aachen, the unit is intended primarily for small and medium-sized enterprises and will cost around €30,000.

Employing a Cartesian coordinate system, the first functional prototype of the new system uses a 140 W laser diode with a focus diameter of 250 µm to produce complex metal components with a maximum height of 90 mm and a maximum diameter of 80 mm. The machine’s footprint measures 1.3 m x 0.8 m x 1.4 m.

According to Dawid Ziebura, Project Engineer at Fraunhofer ILT a unit with a comparable installation space would cost at least €100,000, whereas the FH Aachen/Fraunhofer ILT SLM unit will retail for €30,000. The unit is said to be easy to use, with entry-level users only requiring a few hours to learn how to operate it. All of the components in the sytem allow users to maintain the unit themselves and are easy to replace. “The low-cost unit makes it easy for entry-level users getting into 3D printing of metal components,” Ziebura added.

New low cost system offers easy access to metal Additive Manufacturing

The exposure process in action (© Fraunhofer ILT, Aachen, Germany)

The components that the unit can produce are suitable for many typical SLM applications, ranging from prototypes and sample parts to functional components. Users can select the speed and the production quality at which the unit operates. It was stated that the system can produce a medium-sized (55 cm³), stainless steel part at a density of more than 99.5% within 12 hours.

In addition, the unit offers the option of producing lattice structures for large-volume areas in order to shorten the construction time of less stressed areas. Selecting a lattice density of 20% (corresponding to 20% of the original volume) reduces construction time by 60%.

The engineers in Aachen now want to shorten process times and optimise exposure strategies in order to improve component quality. They are also planning to manufacture components made of aluminium alloys and tool steel.

The new low-cost SLM unit can be seen in action at the Fraunhofer booth at formnext: Hall 3.1, Booth E60.

www.ilt.fraunhofer.de

News
November 7, 2016

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap