Optimised metal powders key to success of precision additively manufactured components

MBFZ Toolcraft GmbH, based in Georgensgmund, Germany, is a specialist manufacturer of high-end precision metal parts and components. The company offers a comprehensive manufacturing service, which includes Additive Manufacturing (metal laser melting), to produce micro-components of the highest dimensional accuracy to meet the demands of a wide range of industries including, biomedical, defence and motor sport.

Many of Toolcraft’s customers are in the medical technology and aerospace sectors, which require the use of certified materials. For applications in these industries, a secure supply of certified powders and the ability to produce components to extremely precise specifications are essential.

The company recently reported that it has been using LPW Technology, Daresbury, UK, to provide powders for these exacting AM applications.  “LPW are ahead of other suppliers in terms of the way in which they analyse powders under the conditions needed to provide relevant data for AM. They also understand how to use these data to help us identify an optimised powder for a specific AM application. LPW not only provide the powders best suited to our needs, but also ensure a secure supply, at an affordable price,” stated Christoph Hauck, Managing Director of Toolcraft.

lpw

Powder analysis at LPW Technology

The properties of the metal powders used directly impact the efficiency of AM processes and, crucially, the mechanical properties of the finished component. To ensure powders are of the highest quality LPW has developed the capability to characterise powders fully. Powders are therefore optimised for Additive Manufacturing. This ability can enhance consistency, quality and significantly reduce costs by managing the degradation of the powders during use in Additive Manufacturing machines.

www.lpwtechnology.com

www.toolcraft.de  

 


Subscribe to our FREE e-newsletter

Your email address:


Useful links:  News | Articles | Introduction to metal Additive Manufacturing


TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap