Circular Refining develops AM electrodes for ammonia-to-hydrogen electrolyser

ApplicationsNews
November 26, 2026
Circular Refining’s Rune Breaker ammonia-to-hydrogen electrolyser incorporates additively manufactured Inconel 718 gyroid electrodes designed to increase the active electrochemical surface area and facilitate gas bubble removal (Courtesy Circular Refining)
Circular Refining’s Rune Breaker ammonia-to-hydrogen electrolyser incorporates additively manufactured Inconel 718 gyroid electrodes designed to increase the active electrochemical surface area and facilitate gas bubble removal (Courtesy Circular Refining)

Circular Refining, Manchester, UK, has developed an additively manufactured electrode architecture for Rune Breaker, its point-of-use liquid ammonia-to-hydrogen electrolyser, in collaboration with the University of Manchester’s School of Engineering under Dr Kamal Qazi.

The development focused on reactor geometry and scalable UK manufacturing, addressing the gas bubble entrapment and high precious metal costs associated with conventional flat-plate electrodes.

The electrodes are manufactured from Inconel 718 nickel-based superalloy using Laser Beam Powder Bed Fusion (PBF-LB). The triply periodic minimal surface (TPMS) gyroid lattice geometry is designed to maximise the active electrochemical surface area and facilitate rapid gas bubble removal.

The anode is electroplated with a catalyst comprising 75% platinum (Pt) and 25% ruthenium (Ru), intended to accelerate electron transfer while minimising precious metal loading.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The electrolyser features an asymmetrical cell configuration comprising three cathodes and one anode, with a polyether ether ketone (PEEK) bubble sheath for gas isolation. The cell is housed within a 316 stainless steel vessel, which reportedly underwent structural testing to a safety factor of 4.742 at a continuous pressure of 20 bar.

The modular electrolyser is intended to demonstrate how UK Additive Manufacturing and materials science can support the production of durable electrochemical hardware at scale. Physical laboratory trials are planned for late 2026 and early 2027.

www.circularrefining.co.uk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
November 26, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap