Rolls-Royce explores Norsk Titanium’s RPD Additive Manufacturing for civil aerospace engines

ApplicationsNews
November 9, 2026
Norsk Titanium has received a purchase order from Rolls-Royce for a Ti-6Al-4V structural component manufactured using its Rapid Plasma Deposition technology (Courtesy Norsk Titanium AS)
Norsk Titanium has received a purchase order from Rolls-Royce for a Ti-6Al-4V structural component manufactured using its Rapid Plasma Deposition technology (Courtesy Norsk Titanium AS)

Norsk Titanium AS, Hønefoss, Norway, has received a purchase order from Rolls-Royce plc for a titanium component being considered for potential use across its current civil aerospace engine programmes.

The Ti-6Al-4V structural component was manufactured at Norsk Titanium’s Technology Center in Norway using the company’s proprietary Rapid Plasma Deposition (RPD) technology. Final machining is being completed in Germany through the project supply chain.

The order forms part of Norsk Titanium’s ongoing work with Rolls-Royce to explore the application of wire-based Directed Energy Deposition (DED) in aerospace engines.

“This order represents an important step forward in our relationship with Rolls-Royce,” said Fabrizio Ponte, President and CEO of Norsk Titanium. “It demonstrates both the maturity of our RPD technology and our ability to work within an established aerospace engine supply chain. We believe this phase of exploratory work creates a foundation for identifying additional development opportunities over time.”

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Norsk Titanium is an approved supplier of parts for Rolls-Royce development activities. The companies will use experience gained through the project to assess potential future applications of RPD technology.

www.norsktitanium.com

www.rolls-royce.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
November 9, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap