Additive Manufacturing Of Inconel 625 Superalloy Produced By Electron Beam Melting
Chauvet, E; Martin, G; Blandin, J J; Dendievel, R (Simap Grenoble France) Vayre, B; Abed, S (PolyShape France)
Characterisation Of EBM-built Shelled Samples Of Ti6Al4V Compacted By HIP
Frisk, K (Alloy Development Sweden) Rännar, L E; Koptyug, A (Mid Sweden University Sweden) Persson, D (Swerea KIMAB Sweden) Vattur Sundaram, M (Chalmers University of Technology Sweden) Ahlfors, M (Quintus Technologies Sweden)
Investigation Of Sintering Parameters On Ti6Al4V Powder For Electron Beam Melting Process Variation
Drescher, P; Seitz, H (University of Rostock Germany)
Effect Of Thermal Treatment Conditions In Mechanical Properties Of Ti6Al4V Parts Manufactured By Selective Laser Melting
Mancisidor, A M; Álvarez, P; Garciandia, F (Ik4-Lortek Spain)
Poster
Instabilities And Ablation Under Laser Melting Of Powder Layers
Chivel, Y (MerPhotonics France)
Session 36: AM – Powder Characteristics
Evaluating Flowability Of Additive Manufacturing Powders, Using The Gustavsson Flow Meter
Mellin, P (Swerea KIMAB Sweden) Lyckfeldt, O (Swerea IVF Sweden) Harlin, P (AB Sandvik Materials Technology Sweden) Brodin, H (Siemens Industrial Turbomachinery AB Sweden) Blom, H (Carpenter Powder Products AB Sweden) Strondl, A (Swerea KIMAB Sweden)
Powders For Additive Manufacturing
Kloeden, B; Kirchner, A; Weißgärber, T; Kieback, B (Fraunhofer IFAM Dresden Germany)
Effect of Process Gas And Powder Quality On AlSiMg And Ti64 Powder Bed Fusion Processed Parts For The Aerospace Industry
Foret, P (The Linde Group Germany) Bauer, D (Airbus Group Innovation Germany)
Effects Of Powder Attributes And Direct Metal Laser Sintering (DMLS) Process Conditions On The Microstructure And Mechanical Properties Of 17-4 PH Stainless Steel
Atre, S; Irrinki, H (University of Louisville United States)
Session 43: AM – Properties of Lightweight Materials II
Additive Manufacturing Of Magnesium Alloy Powders: Investigations Into Process Development Using Elektron®WE43 And Elektron®21 Via Laser Powder Bed Fusion And Directed Energy Deposition
Tandon, R (Magnesium Elektron Powders United States) Palmer, T (Pennsylvania State Univeristy United States) Gieseke, M; Noelke, C; Kaierle, S (Laser Zentrum Hannover e.V. Germany)
Water Polishing Of Ti6Al4V Manufactured With Electron Beam Melting Technology
Rännar, L E; Koptyug, A; Bäckström, J (Mid Sweden University Sweden) Jönsson, A (Swedish Waterjet Lab Sweden)
Surface Finishing, And Characterization Of Titanium Additive Manufacturing Components: From Rich To Smooth Textures
Diaz, A (REM Surface Engineering United States)
As-HIP Microstructure Of EBM Fabricated Shell Components
Leicht, A; Vattur Sundaram, M; Hryha, E; Nyborg, L; (Chalmers University of Technology Sweden) Ahlfors, M (Quintus Technologies AB Sweden) Rännar, L E; Koptioug, A (Mid Sweden University Sweden) Frisk, K (Swerea KIMAB AB Sweden)
Development Of A Metal 3D Printer Using Laser Powder Deposition And Process Optimization For Fabricating Titanium Alloy Parts
Jeong, W (POSTECH Korea, Republic of) Kang, M G (Cetatech Inc. Korea, Republic of) Kim, D (POSTECH Korea, Republic of) Kwon, Y S (Cetatech Inc. Korea, Republic of)
Application Of Rare Earth Elements In Additive Manufacturing
Li, I (Material Technology Innovations Co. Ltd. China) Yang, A (MTI China)
Titanium-based Permeable Coatings Produced By Selective Laser Sintering Spherical Titanium Powders
Grigoriev, E (NRNU MEPhI Russian Federation) Ilyuschenko, A; Kuznechik, O; Bykov, R (Powder Metallurgy Institute Belarus)
Microstructures and Mechanical Properties of Ti-6AI-4V Thin Plates by SEBM
Wang, J; Tang, H; Liu, N; Yang, K; Song, C; Jia, L (Northwest Institute of Nonferrous Metal Research, China) Liu, Y (Northwest Institute of Nonferrous Metal Research, China /Central South University, China)
Session 50: AM – Special Aspects in AM Technology
Component Scale Process Model For Metal Additive Manufacturing
Andersson, T; Laukkanen, A; Pinomaa, T (VTT Materials and Manufacturing Finland)
Optical Monitoring And Control Of The Surface Thermal Processes
Chivel, Y (MerPhotonics France)
3D Screen Printing – Additive Manufacturing Of Finely Structured Titanium Based Parts
Jurisch, M; Studnitzky, T; Andersen, O; Kieback, B (Fraunhofer IFAM Germany)
Additive Technology Of Ceramic Turbomachine Manufacturing
Chivel, Y (MerPhotonics France) Sudarev, A; Konakov, V (Ceramic & Glass LTD Russian Federation)
Session 51: AM – Special Powder and Materials
Selective Laser Melting Of Steel-based Metal Matrix Composites With Ceramic Reinforcement
Castro, F (CEIT Spain) Martinez, E; Niñerola, R; (AIMME Spain) Sainz, S (CEIT Spain)
Microstructural And Mechanical Properties Of Al-Si-Ni-Ce Alloy Produced By Direct Metal Laser Sintering
Aversa, A (Politecnico di Torino Italy) Lorusso, M; Trevisan, F; Manfredi, D; Calignano, F (Istituto Italiano di Tecnologia Italy) Biamino, S (Politecnico di Torino Italy) Ambrosio, E (Istituto Italiano di Tecnologia Italy) Fino, P; Pavese, M (Politecnico di Torino Italy)
Microstructures And Mechanical Properties Of Selective Laser-melted Metals With Different Processed Powder
Nomura, N; Kikuchi, K; Kawasaki, A (Tohoku University Japan)
Study Of Single Tracks With AlSi10Mg And Composites Powders
Librera, E; Aversa, A; Moshiri, M; Fino, P; Biamino, S; Lombardi, M; Pavese, M; Manfredi, D; Calignano, F; Ambrosio, E; Lorusso, M (Istituto Italiano Tecnologia Italy)
Poster
New Low-density Composite Powder For Powder Metallurgy And Additive Manufacture
Shishkin, A (Riga Technical University Latvia)