ORNL researchers use neutrons to discover strengthening behaviour in additively manufactured alloys
Researchers at Oak Ridge National Laboratory (ORNL), Tennessee, USA, are reported to have identified a mechanism in an additively manufactured alloy, termed load shuffling, that could enable the design of ... Read more »