PyroGenesis ships first commercial samples of NexGen plasma-atomised titanium AM powder
PyroGenesis Canada, Inc, Montreal, Québec, Canada, reports that since starting operation of its Additive Manufacturing NexGen™ powder production line, it has now shipped its first commercial samples ... Read more »