AML3D to manufacture prototype parts for Royal Australian Navy’s Hunter class frigates

ApplicationsNews
December 5, 2023
AML3D will produce prototype parts for use in the new Hunter class frigates for the Royal Australian Navy (Courtesy AML3D)

AML3D Limited, located in Edinburgh, Australia, has signed a prototype part manufacture and testing contract with BAE Systems Maritime Australia (BAESMA). The prototype part is a test component for use within BAESMA’s contract to design and build the Hunter class frigates for the Royal Australian Navy.

The announcement follows feasibility and commercial validation testing programmes that reportedly demonstrated AML3D’s Wire Arc Additive Manufacturing (WAAM) as a cost-effective manufacturing solution that meets the standards of the Royal Australian Navy.

The contract will be fulfilled at AML3D’s manufacturing facilities in Adelaide and is expected to last for eight to ten weeks.

In addition to expanding AML3D’s relationship with BAESMA, the contract also highlights the potential role of AML3D’s Wire Arc Additive Manufacturing technology in bolstering Australia’s sovereign manufacturing capability, which could be applicable to other markets.

“We had great confidence that our WAM technology would satisfy BAESMA’s testing and move into component manufacturing,” stated Sean Ebert, AML3D’s Chief Executive Officer. “AML3D has a focus on the significant demand we are seeing in the US, where we are enjoying a lot of success in winning a steady stream of contracts, but we also have a stated aim to develop our commercial relationships across additional marine and defence sectors. Expanding our relationship with BAESMA in Australia, as part of its work for the Royal Australian Navy, is a great example of delivering on this aspect of our growth plan and diversifying our revenue base.”

www.aml3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
December 5, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap