SPEE3D demonstrates its ACTIVAT3D copper coating process as interest grows

SPEE3D has replaced existing door handles within Australia’s Northern Territory Department of Trade, Business and Innovation with ACTIVAT3D copper (Courtesy SPEE3D)

SPEE3D, headquartered in Melbourne, Australia, demonstrated its ACTIVAT3D copper coating process during a live online presentation. The company recently announced the successful development and testing of ACTIVAT3D copper, a fast and affordable way to additively manufacture anti-microbial copper onto existing metal surfaces.

In addition to the live demonstration, SPEE3D also reports that the Northern Territory Department of Trade, Business and Innovation has become the first organisation to deploy antimicrobial ACTIVAT3D copper throughout their building, to help fight the spread of coronavirus (COVID-19).

SPEE3D states that it was contracted to replace existing door handles within the Northern Territory Department of Trade, Business and Innovation with ACTIVAT3D copper products. With these handles now installed, the company states that the staff of this department, and the community they interact with, are already experiencing the benefits of antimicrobial copper.

Shaun Drabsch, Department of Trade, Business and Innovation CEO, stated, “The Department of Trade, Business and Innovation is thrilled to be the first to have this innovative technology installed in our workplace, ensuring an even safer place for our staff and community to do business here. We thank our landlord for agreeing to the installation of copper handles. It is great to see a local Territory company taking advantage of this very challenging time and drive a new innovative product that can further protect Territorians from COVID-19.”

According to SPEE3D, the lab results have sparked global interest in its technology as governments and private companies look for proactive ways to protect their communities. With this technology now proven and enquiries coming in from around the world, the company states that it is looking to partner the door handle manufacturing industry to deliver ACTIVAT3D copper at scale to where it is needed most.

www.spee3d.com

https://business.nt.gov.au


SPEE3D features in the Spring 2020 issue of Metal AM magazine: ‘Cheaper powders, faster build speeds and no thermal stresses? How AM is going supersonic at SPEE3D’. Read the article in full here.


TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap