AmPd Labs, based in Houston, Texas, USA, has published a white paper investigating how Hot Isostatic Pressing (HIP) and heat treatment can improve the mechanical properties of MAR-M 247LC, a nickel-base superalloy processed using Binder Jetting (BJT). The alloy is a low-carbon derivative of MAR-M 247, developed for high-temperature turbine components.
The paper builds on the company’s April 2026 study, which demonstrated room-temperature mechanical properties comparable to published data for conventionally cast MAR-M 247 but identified limitations in yield strength, hardness and residual porosity.
Test specimens were manufactured using a Desktop Metal Shop System and gas-atomised MAR-M 247LC powder supplied by Continuum Powders. Testing was conducted by accredited independent laboratory Accu-Test Labs.

The white paper highlights several findings across the different processing routes:
- Porosity elimination: A newly developed sintering cycle, designated the ‘03 Procedure’, followed by HIP, reduced measured porosity from 5.6–8.8% to zero in the metallographic sections examined.
- Increased tensile strength: Following the 03 Procedure and HIP, average room-temperature ultimate tensile strength reached 1,312 MPa, approximately 19% above the April 2026 baseline and 33% above the published benchmark for cast, HIPed and heat-treated MAR-M 247.
- High ductility: The same processing route achieved an average elongation of 17.5%, approximately 2.6 times that of the cast benchmark.
- Improved yield strength: A separate processing route using the original sintering cycle followed by HIP, annealing and ageing achieved a yield strength of 858 MPa, comparable to conventionally cast, HIPed and heat-treated MAR-M 247.
- Improved manufacturability: The new sintering cycle was developed to overcome dimensional instability, distortion and cracking encountered with the original process.
- Grain size: HIP following the 03 Procedure eliminated measurable porosity without measurable grain growth, retaining an average grain diameter of approximately 22 µm.
- Improved hardness: Both HIP processing routes achieved hardness values of 36.3–37.5 HRC, within the published cast material range of 35–40 HRC.

AmPd Labs is conducting creep and stress-rupture testing at 760°C (724 MPa) and 982°C (200 MPa) to evaluate the suitability of the material for high-temperature applications. The white paper notes that the fine grain structure achieved through BJT and subsequent processing could limit creep life compared with coarse-grained cast material.
Further testing is also needed to establish repeatability, with the reported tensile results for the two HIP processing routes based on two specimens and a single specimen, respectively.