Apex first UK company to be awarded ASTM’s AMC-QS quality certification

News
November 25, 2026
Apex Additive Technologies, which operates Renishaw RenAM 500Q Additive Manufacturing machines at its facility in Ebbw Vale, Wales, was the first UK company to achieve ASTM’s AM Quality System Certification (Courtesy ASTM)
Apex Additive Technologies, which operates Renishaw RenAM 500Q Additive Manufacturing machines at its facility in Ebbw Vale, Wales, was the first UK company to achieve ASTM’s AM Quality System Certification (Courtesy ASTM)

Apex Additive Technologies, based in Ebbw Vale, Wales, has achieved AM Quality System Certification (AMC-QS) from ASTM International’s Additive Manufacturing Center of Excellence (AM CoE). The company was the first in the UK to achieve the recognition.

Apex specialises in Laser Beam Powder Bed Fusion (PBF-LB), operating multi-laser AM machines alongside in-house heat treatment, finishing and materials characterisation capabilities. According to ASTM’s AM CoE, the certification reflects several years of investment in manufacturing practices and the development of Apex’s own electronic quality management system.

The certification evaluates an organisation’s overall quality management system from an AM-specific perspective, including material management, process control, production consistency and traceability.

The scheme applies across AM processes and materials, rather than certifying one manufacturing process or component.

AMC-QS builds on existing quality management certifications, such as ISO 9001 and AS9100, and draws on several ISO/ASTM standards covering Additive Manufacturing quality requirements. Certification is valid for three years, subject to annual surveillance audits.

Apex achieved ISO 13485 certification in September 2026. AMC-QS provides an additional level of assurance for customers requiring controlled and repeatable AM production.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Other organisations to have achieved AMC-QS certification include KSB, AM Craft, Additive Manufacturing Solutions and the National Center for Additive Manufacturing Excellence (NCAME) at Auburn University.

www.apex.tech

www.amcoe.org

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

News
November 25, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap