ITACAe uses metal Additive Manufacturing to reduce cooling block weight by 41%

Italian engineering company ITACAe, based in Asti, showcased an additively manufactured refrigeration block at Vehicle & Transportation Technology Innovation Meetings (VTM) Torino 2026, held November 23–25. The block was designed for S.P.M. S.r.l., a manufacturer of polyurethane processing machinery based in Cassolnovo, Italy.
The component forms part of a robotic-arm-mounted mixing head used in two-component polyurethane production. It was manufactured in AlSi10Mg using Laser Beam Powder Bed Fusion (PBF-LB).

The project achieved a 41% reduction in component weight, from 1.45 kg to 0.86 kg, and aimed to improve cooling performance through optimised internal cooling channels.
The component was developed as part of the OPTIPOMIX project, supported by the Pulsate Network, a European initiative established to encourage the industrial adoption of laser-based manufacturing technologies.