DN Solutions and Addiguru demonstrate AM defect detection at Formnext

DN Solutions, Changwon, South Korea, and Addiguru, New Orleans, Louisiana, USA, are demonstrating automated defect detection at Formnext 2026 using build data from a DN Solutions DLX metal AM machine. The demonstration focuses on identifying potential defects earlier in the manufacturing process, with the aim of reducing the time and costs associated with subsequent processing and inspection.
Building on decades of experience in CNC machining, DN Solutions expanded into metal Additive Manufacturing with its DLX series of Laser Beam Powder Bed Fusion (PBF-LB) machines, providing opportunities to integrate additive and subtractive manufacturing processes.

The companies state that post-build operations can account for 30–50% of the cost of an additively manufactured component. Defects identified only after heat treatment, CNC machining and final inspection can therefore result in significant additional costs.
At Formnext, Addiguru’s automated in-situ monitoring platform analyses individual layers of the powder bed via images recorded during a build on a DN Solutions DLX machine. The software identifies potential defects and tracks them throughout the build.
Manually reviewing thousands of layer images can require hours of engineering time. Addiguru’s platform highlights areas of concern and can notify users when potentially critical issues are detected.
For manufacturers producing high-value components, earlier identification of potential defects could help avoid unnecessary machining and inspection. This is particularly relevant where computed tomography (CT) scanning or other costly non-destructive inspection methods are required. In-situ monitoring is not intended to replace established quality assurance processes, but can provide information to help determine where further investigation may be necessary.

Following Formnext, DN Solutions and Addiguru are evaluating the integration of additional sensor and machine data alongside the powder bed images.
“A defect found during the build costs a reprint. Found after five-axis finishing and CT, it costs the reprint plus every machine hour and inspection that went into the part,” stated Dr Vino Suntharakumaran, Vice President Additive Manufacturing at DN Solutions. “We want that information as early as possible, in the same workflow that takes a preform to a finished part. Formnext is where we start testing this with Addiguru.”
Shuchi ‘SK’ Khurana, CEO of Addiguru, added, “The value is quite simple. If we can identify a potential problem during the build, why wait until after machining and expensive inspection to find it? DN Solutions already understands the complete journey from Additive Manufacturing through to the finished component. By bringing our monitoring technology into that process, we help manufacturers find problems earlier, make better decisions and avoid unnecessary cost.”