AMAZEMET to show laser ultrasonic atomiser at Formnext

Amazemet will present a new standalone laser ultrasonic atomiser at Formnext 2026 (Courtesy Amazemet)
Amazemet will present a new standalone laser ultrasonic atomiser at Formnext 2026 (Courtesy Amazemet)

Amazemet, Warsaw, Poland, will present a new standalone laser ultrasonic atomiser at Formnext 2026, taking place in Frankfurt from November 17–20. Combining focused laser melting with ultrasonic atomisation, the machine is designed to produce metal powders for materials research.

The process uses a laser beam focused on metal feedstock to create a melt pool on an ultrasonic element, known as a sonotrode. Vibrations from the sonotrode break the molten metal into droplets, which cool and solidify to form powder. The laser provides the heat, while the ultrasonic element is responsible for atomisation.

According to Amazemet, the use of laser melting allows the machine to process a range of materials, from aluminium, typically melted using induction heating before atomisation, to high-melting-point metals that can also be processed using the company’s rePOWDER plasma module.

Laser heating also eliminates a potential source of tungsten contamination associated with consumable electrodes and can help limit unwanted evaporation of alloying elements.

SEM images and particle size distributions of molybdenum, tungsten, aluminium and Ti6Al4V powders (Courtesy Amazemet)
SEM images and particle size distributions of molybdenum, tungsten, aluminium and Ti6Al4V powders (Courtesy Amazemet)

The standalone machine incorporates a 3 kW laser and offers operating cycles of up to four hours for aluminium and titanium when using established process parameters. Production rates and operating durations vary depending on the material and process conditions.

Powders produced using laser-based ultrasonic atomisation include molybdenum, tungsten, aluminium and Ti6Al4V. Scanning electron microscopy (SEM) images show the particle morphology of these powders, alongside corresponding particle size distributions for each sample.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Amazemet is exhibiting in Hall 12.0, Booth D42, where visitors will be able to observe ultrasonic atomisation in operation and discuss the machine’s capabilities, materials, research objectives and powder requirements with the company’s technical and sales team.

www.amazemet.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap