Renishaw and ITP Aero advance AM for aerospace with certified parts

The Tail Bearing Housing additively manufactured via Renishaw’s Additive Manufacturing technology (Courtesy ITP Aero)
The Tail Bearing Housing additively manufactured via Renishaw’s Additive Manufacturing technology (Courtesy ITP Aero)

Renishaw, based in Wotton-under-Edge, Gloucestershire, UK, and aircraft engine manufacturer ITP Aero, Zamudio, Spain, recently highlighted the progress made on their journey towards using Additive Manufacturing to process nickel-based and lightweight alloys, as well as high-temperature materials.

Working together since 2016, the companies’ original knowledge and resource-sharing agreement evolved into a strategic technological alliance that focuses on the development of processes, standards and certified components.

“Renishaw has always shared with us its experience accumulated with other customers and sectors, understanding the particularities of each alloy and thus enabling us to accelerate the development process,” stated Fernando Lartategui, Associate Researcher in Additive Layer Manufacturing at ITP Aero.

According to the companies, this transfer of knowledge has been essential for developing components such as the Tail Bearing Housing (TBH), one of the two joining elements between the aircraft and the Rolls-Royce UltraFan engine — reportedly the largest in the world. The engine, scheduled for launch at the end of the decade, is intended to be compatible with 100% sustainable aviation fuels and reportedly offers a 25% fuel efficiency improvement compared to the original Trent 700 model.

Certified components

ITP Aero has produced the TBH using Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing. Renishaw’s Solutions Centre in Barcelona contributed its experience in build preparation and execution, including scanning strategies, parameter development and layout optimisation.

The collaboration between Renishaw and ITP Aero has also contributed to the manufacture of already certified and in-production aerospace components, such as the TP400 engine vanes of the rear engine structure. According to the companies, these were the first structural components produced by PBF-LB Additive Manufacturing to be certified by both the European Union Aviation Safety Agency (EASA) and the Spanish Aviation Safety and Security Agency (AESA).

Working alongside Renishaw has also enabled ITP Aero to establish its own internal Additive Manufacturing standards, including specifications and process regulations. This standardisation provides technical consistency and traceability.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

€24 million for advanced manufacturing

ITP Aero has also created a new advanced manufacturing centre inaugurated with an investment of €24 million In February 2025. Located at the company’s headquarters in Zamudio and using AM as one of the four pillars of R&D activity, the centre aims to develop solutions for more sustainable aircraft engines and improve manufacturing process efficiency amongst other goals.

Precise tuning of laser parameters

In an effort to further improve AM, Renishaw has developed Libertas, a flexible framework that gives freedom to precise tuning of laser parameters, tailored to the requirements of individual applications.

“Traditionally, support structures are required for surfaces with a critical angle of 45º or more from the horizontal. With the Support Reduction Package, this threshold has been extended—reducing the critical angle to as little as 5º in certain cases,” explains Benjamin Díaz, Additive Manufacturing Product Manager at Renishaw Ibérica. “Beyond reducing support requirements, this approach also enhances surface finish and mitigates thermal stress by intelligently regulating energy distribution during the build process.”

At Formnext, Renishaw will present a preview of Libertas at its Hall 11.0, C11 booth alongside a complete end-to-end AM cell, a new long-life filtration system for the RenAM 500 series, and Argive’s high-performance microturbine.

www.renishaw.com

www.itpaero.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap