Markforged adds pure copper to its Metal X rapid Additive Manufacturing system
Markforged, Watertown, Massachusetts, USA, has added pure copper to the range of materials processable by its Metal X rapid Additive Manufacturing system. The company stated that the inclusion of copper ... Read more »