Scandium Canada reports crack-resistant Al-Sc alloys for Additive Manufacturing
Scandium Canada Ltd, headquartered in Montreal, has reported new data on its modified AA535 and AA7075 aluminium-scandium (Al-Sc) alloys. When processed via Laser Beam Powder Bed Fusion (PBF-LB), these alloys ... Read more »