Avimetal showcases recycled Ti-6Al-4V powder and MT400M metal AM machine at Formnext

Avimetal, Beijing, China, is showcasing its latest 100% recycled Ti-6Al-4V titanium alloy powder at Formnext 2026. At Hall 11.0, stand D21, the company is presenting titanium Additive Manufacturing materials, equipment and process technologies to visitors from Europe and other international markets.
Avimetal has developed a recycling process for Ti-6Al-4V titanium alloy coarse powder and titanium machining scrap. The process covers powder recovery, oxygen reduction control, EIGA atomisation, sieving and inspection, with the company reporting a 100% regeneration rate. The company reports an annual production capacity of 1,800 tonnes of recycled Ti-6Al-4V powder.

The recycled Ti-6Al-4V powder is available in particle size ranges of 0–20 µm and 15–53 µm. According to Avimetal, the powder offers good flowability and produces dense components with batch-to-batch consistency comparable to virgin atomised powder. The material is suitable for processes including Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing and Metal Injection Moulding (MIM).
The powder is already being supplied in volume, primarily for the production of lightweight precision components for the global consumer electronics market. Avimetal states that its use can help customers reduce material costs, improve supply chain sustainability and meet environmental, social and governance (ESG) objectives.

Alongside its recycled powder, Avimetal is exhibiting its wider portfolio of titanium AM materials, equipment and process technologies.
The company produces fine spherical titanium alloy powders using technologies including AVI-EIGA, plasma atomisation (PA) and plasma spheroidisation (PS), alongside its recycling process. It reports established volume production of titanium alloy powders, with Ti-6Al-4V, BT20, CP Ti and TC11 among the materials being displayed at Formnext. These powders are intended for applications requiring lightweight, high-strength precision components.

Avimetal has also developed the MT400M and MT400S series of metal AM machines. Features include multi-laser configurations, 60/80 µm laser spot sizes, ring beam shaping and the ability to process larger layer thicknesses. The company states that these developments are intended to improve build efficiency and component quality. A live demonstration of the MT400M is taking place at its stand.
Using the MT400M series and Ti-6Al-4V powder, Avimetal reports having validated full-build-plate batch production of 24 automotive connecting brackets in 144 hours and 2,248 mobile phone hinge shaft caps in 60 hours. According to the company, the manufactured components met the required performance criteria, demonstrating the equipment’s potential for batch production.
Examples of these batch-produced titanium components are also on display at Formnext.