Equispheres and Aconity3D boost productivity using laser beam shaping and NExP-1 powder

EquipmentMaterialsNews
November 9, 2023
Equispheres and Aconity3D have reported achieving metal AM build rates up to nine times greater than is typical (Courtesy Equispheres Inc)
Equispheres and Aconity3D have reported achieving metal AM build rates up to nine times greater than is typical (Courtesy Equispheres Inc)

Equispheres, Inc, Ottawa, Ontario, Canada, and Aconity3D, Herzogenrath, Germany, have reported achieving metal Additive Manufacturing build rates up to nine times greater than is typical for aluminium powder and Laser Beam Powder Bed Fusion (PBF-LB) AM processes.

Building on previous announcements of production speeds around three times faster than is norm, Aconity3D and Equispheres report production speeds in excess of 430 cm3/hr for a single laser. This was achieved using Equispheres’ NExP-1 AM AlSi10Mg powder, and an AconityMIDI+ AM machine with laser beam shaping.

“There are three pillars supporting this remarkable achievement,” stated Evan Butler-Jones, VP – Product & Strategy at Equispheres. “The leading-edge capabilities of Aconity3D’s printing technology, the novel application of beam shaping, and the unique powder properties of Equispheres’ NExP-1 printing material. This powerful combination allowed us to achieve outstanding results.”

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Laser beam shaping is used in other industries and has gained attention in Additive Manufacturing due to its potential to improve processing speeds. In PBF-LB, beam shaping modifies how energy is deposited on the powder bed, altering the power density and thermal gradient.

To fully explore the potential of beam shaping, the two partners selected NExP-1 AM for its stable melting behaviour as well as a tightly controlled Additive Manufacturing process on an AconityMIDI+ modified with an IPG YLR 3000/1000-AM with beam shaping capabilities enabling 3 kW of maximum power. The shaped beam – rather than a zoomed gaussian beam – reduces overheating and spatter formation in high productivity processing.

“Aconity3D’s printing technology and the team’s expertise were crucial to this project’s success. We’re working with extremely high-powered lasers, testing additive manufacturing process parameters far beyond previous capabilities. It was necessary to have the precise control and monitoring capabilities of Aconity3D printers,” says Butler-Jones.

“NExP-1 powder is vital to achieve these remarkable speeds,” explains Martin Buscher, Aconity3D. “It has exceptional properties that make it ideal for high-speed work. The powder characteristics enable optimal melting behaviour, which is required to achieve consistent printing with high-powered lasers at these extraordinary speeds.”

Equispheres and Aconity3D discussed the productivity impacts achieved by combining engineered beam profiles with engineered powders when processes aluminium via PBF-LB Additive Manufacturing at Formnext 2023, on the technology stage. Equispheres is currently exhibiting at Hall 11, B31 and Aconity3D, 12, B42.

www.equispheres.com

www.aconity3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
EquipmentMaterialsNews
November 9, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap