Taniobis and Alloyed receive 2023 Gustaf Ekeberg Award for tantalum research

MaterialsNewsResearch
September 26, 2023
Kazuhiko Iida, CEO of Taniobis, received the Gustaf Ekeberg Award during the General Assembly of the T.I.C. in Rio de Janeiro (Courtesy Taniobis)
Kazuhiko Iida, CEO of Taniobis, received the Gustaf Ekeberg Award during the General Assembly of the T.I.C. in Rio de Janeiro (Courtesy Taniobis)

The authors of ‘Tailored Niobium-Based Alloys for Additive Manufacturing: From Powder Production to Parameter Optimization’, jointly published by Taniobis GmbH, a subsidiary of JX Metals Corporation, headquartered in Goslar, Germany, and Alloyed Ltd, based in Oxford, UK, have been honored with the Gustaf Ekeberg Award.

The Ekeberg Award – named after the discoverer of tantalum, Anders Gustaf Ekeberg – is given to individuals or research teams who have made notable contributions to the processing, properties, and applications of tantalum. This prestigious award, presented by the TIC (Tantalum-Niobium International Study Centre), aims to promote awareness of the exceptional properties and potential applications of tantalum. The award ceremony was held on September 11 during the 64th General Assembly of the TIC in Rio de Janeiro, Brazil.

The research conducted by Taniobis and Alloyed focuses on the development of customised tantalum- and niobium-based alloy powders for Additive Manufacturing. Alloys like AMtrinsic® C103 and AMtrinsic FS-85 are said to be particularly intriguing due to their relatively low density, good thermal conductivity, and impressive temperature and time-dependent mechanical properties. These properties are especially valuable when Ni- and Co-based superalloys face limitations at temperatures above approximately 1050°C.

While C103 is widely used in traditional manufacturing methods, the alloy FS-85, which contains tantalum, offers superior high-temperature performance and creep resistance at elevated temperatures. However, producing parts using conventional processing methods like casting and machining has always been challenging. The development of commercially available FS-85 alloy powders for Additive Manufacturing has opened up opportunities for new, high-value applications involving complex-shaped, high-performance components. To successfully develop such powders, it is necessary to understand the workflow from powder production and characterisation to determining the optimal process parameters. In the awarded paper, Taniobis and Alloyed provide a detailed account of the process of preparing, characterising, and processing two alloy powders – C103 and FS85 – using metal AM.

“We thank Alloyed for the outstanding collaboration, now being recognised with this award. Taniobis GmbH is proud of this achievement and sincerely thanks TIC for recognising our commitment to advancing tantalum research and innovation. The collaboration with Alloyed opens new possibilities for high-performance and high-temperature applications in Additive Manufacturing technology, benefiting numerous industries,” stated Kazuhiko Iida, CEO, Taniobis.

www.taniobis.com

www.alloyed.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
September 26, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap