Patent granted for use of oxalic acid powder for debinding POM feedstocks

MaterialsNews
August 14, 2023
The patented catalytic debinding solution from XERION Berlin Laboratories GmbH uses oxalic acid powder in a separately heated powder cartridge

XERION Berlin Laboratories GmbH, Berlin, Germany, has announced a patent for a new method for catalytically debinding polyoxymethylene (POM) based feedstocks, such as BASF’s Catamold® for Metal Injection Moulding (MIM) or its Ultrafuse® filaments for Additive Manufacturing, using oxalic acid powder.

Both the Catamold and Ultrafuse materials see widespread use in MIM and metal Fused Filament Fabrication (FFF, also known as filament-based Material Extrusion (MEX)) thanks to the reduced time required for catalytic debinding compared to solvent based debinding methods. This is especially the case for parts with larger wall thicknesses and allows for faster batch processing and higher throughput for manufacturers.

Typically, nitric acid in varying concentrations is used to catalytically debind POM-based feedstocks in order to remove the polymer backbone before sintering. While advantageous for the aforementioned reasons, the challenges that nitric acid poses with regard to the environment, as well as safe handling, are well known within the industry. The new catalytic debinding method from XERION, used in its Fusion Factory XS system, alleviates these issues by using oxalic acid rather than nitric acid.

Oxalic acid is naturally occurring, found in various plants, leaves and even honey. As opposed to nitric acid, which is stored as in liquid form, oxalic acid can be stored as an odourless powder, which is safe to handle. It was stated that the amount of oxalic acid required for catalytic debinding in the Fusion Factory XS is comparable to the amount of oxalic acid that one would find in a handful of rhubarb leaves. The byproducts from the use of oxalic acid in the Fusion Factory XS system from XERION Berlin Laboratories present no harm to the environment and processing time is similar to debinding with nitric acid.

The Fusion Factory XS is an all-in-one metal FFF Additive Manufacturing, debinding and sintering system, built into multiple compact Pelican™ cases that are easily transported and can endure rugged conditions. The debinding unit and sintering furnace are housed together within one Pelican case, where the catalytic debinding unit consists of two independently heated interconnected chambers. Within the box chamber, ‘green’ AM or MIM parts are placed where they are heated to an elevated temperature.

The other chamber contains a pre-prepared oxalic acid cartridge, which is then heated so that the oxalic acid sublimates and is transported to the chamber with the green parts. The remnants of moved backbone polymer are then safely burned off within an electrical burner, therefore posing no risk to anyone in the vicinity of the system.

The sintering furnace can achieve temperatures up to 1,550°C within an argon/forming gas atmosphere. The furnace utilises a cold-wall system, cooled by a chiller housed within a separate Pelican case. During thermal debinding, the same electrical burner as the debinding unit is used.

The custom-made dual extruder AM machine, specifically designed for the processing of powder-filled POM filaments, is housed within its own Pelican case. Filament is stored on compact spools that move on an independent linear rail, as part of a separate patent belonging to XERION. The overall solution therefore lends itself well to BASF Ultrafuse stainless steel in combination with its ceramic support interface.

XERION stated that it has considered the safety and environmental impact in every aspect of the Fusion Factory XS system, with its compact and transportable footprint enabled by this new method of catalytic debinding using oxalic acid.

www.xerion.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
August 14, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap